Conductive Coatings And Future Requirements In Vehicle Glass Design

New printed electric circuits and higher voltage supply will influence conductive coatings for vehicle glass. In this paper the author illustrates the status, opportunities, and challenges for these products.

Author
S Schreiber
Origin
Conductive Coatings
Journal Title
Int Glass Review 3/2000 87-89
Sector
Flat glass
Class
F 1148