A Comparative Analytical Study Of The Origin Of The Art Of Venetian Glassmaking (English And Italian)

Chemical analysis of about thirty Venetian glass finds dated between the 8th and 16th centuries has provided new data on the origins of Venetian glassmaking.

Author
M Verita, T Toninato
Origin
Stazione Sperimentale Del Vetro
Journal Title
Riv Staz Sper Vetro 1990 20 4 169-175
Sector
Domestic glass
Class
D 107