Colored Glass: V, Fluorescence And Solarisation Of Glass.

W. first deals with the fundamentals of fluorescence, the excitation, lifetime, and quenching of fluorescence and the influence of atomic surroundings and then classifies fluorescent glasses on a basis of the role played by the vitreous phase.