Coatings Based On Phosphate Binders

Hydroxyapatite coatings based on phosphate binders are described. Their adhesion characteristics, the TCLE, and the effect of the temperature on the strength of the material of the coatings are presented. Coatings based on phosphate binders can preset interest for specialists in electrochemistry and medicine

Author
V I Vereshchagin Etal
Origin
Tomsk Polytechnical University, Tomsk, Russia
Journal Title
Glass And Ceramics 57 5-6 2000 215 - 218
Sector
General
Class
G 3246