As a direct result of extensive customer feedback concerning the lack of bottle choice in the global wine industry supply chain, Croxsons has taken over a glass furnace at one of the largest glass manufacturers in China to produce antique-green wine bottles aimed specifically at Australia, New Zealand and the US wine markets.