[China] Chinese Approach To Flat Glass And Energy Conservation

The Chinese Government and people attach great importance to problems related to energy saving and emissions reduction, as well as sustainable development. In this article the author sets the scene for China Glass 2010 with a detailed assessment of local energy conservation initiatives and the potential for energy saving flat glass materials.

Author
M Wenyi
Origin
Chinese Ceramic Society, Beijing
Journal Title
Glass Worldwide March-April 2010 68, 70-72, 74-75
Sector
Flat glass
Class
F 2866

Request article (free for British Glass members)