Chemically-Durable Silver Pastes For Heated Windows

Based on a presentation at the 1994 conference of the Society of Glass & Ceramic Decorators, this paper by Alan Caroll describes improvements made to the silver pastes used in the manufacture of heated automotive windows. The pastes are said to be more durable and contain little or no lead.

Author
A Caroll
Origin
Du Pont Electronic Materials, Usa
Journal Title
Glass International June 1995 45-46, 49