The Chemical Analysis Of Lead Crystal Glass

Recommended procedures for the chemical analysis for full lead crystal glass and lead crystal glass are described.

Author
Chemical Analysis Committee Of The Society
Origin
Unknown
Journal Title
Society Of Glass Technology 22 5 1981 201-210