Characterization Of Conventional Silica Superstructure Refractories

Independent creep data on commercial silica refractory materials is now becoming available due to a project at Oak Ridge National Laboratory.

Author
J Hemrick & A Wereszczak
Origin
Unknown
Journal Title
Glass Industry 80 7 June 1999 15-18