Characteristics Of Glass Flow In A 4-Machine System Without Floaters (In Russian)

A model study has been carried out on a model of a 4-machine flat glass tank at the Panevezh glass factory with a particular reference to flow in the forehearth. The advantages of using models for containing furnace design data are discussed.

Author
F.G. Solinov Et Al
Origin
Unknown
Journal Title
Steklo I Keramika 1968 25 (6) 1-4
Sector
Primary Papers
Class
PP 646