Characterisation Of Tin Oxide Films By Complementary Techniques

This paper is a report of the ICG/TC 19 Committee on "Physical Methods for Studying Glass Surfaces". A complete characterisation of tin oxide coatings, deposited on soda-lime glass sheets for industrial applications is presented and the results obtained by different techniques are compared.

Author
C Anderson Et Al
Origin
Unknown
Journal Title
Glass Technology 37 6 1996 204-210