Characterisation And Strucutral Aspects Of Fluorophosphate Glasses

Nine homologous series of fluorine phosphate and one series of pure phosphate glasses of laser glass types have been prepared and characterised by determining the linear and non-linear refractive values and disperation, the glass transition temperature, thermal expansion, density, and anion mole volumina. The results are discussed with respect to structural; aspects.