Change In The Chemical Durability Of Diopside-Containing Silicate Glasses

Acid and alkali resistances of glasses in the albite-diopside, orthoclase-diopside as well as quartz diopside systems were studied. The dependence of property changes on the content of components in glass compositions was investigated. Optimum ratios of compositions are given.

Author
V N Makarov & O V Suvorova
Origin
Unknown
Journal Title
Glass Ceram 54 7-8 1997 235-236
Sector
Special Glass
Class
S 1602a