The Certincoat System

This paper describes the "Certincoat" hot end coating system.

Author
G H Lindner
Origin
Elf Atochem Vlissingen, The Netherlands
Journal Title
Glass Machinery Plants & Accessories Vi 5 1993 53-55
Sector
Container glass
Class
C 576