Central Europe Benefits As Calumite Grows

Calumite sro has been supplying Calumite brand slag to the Central EU glass industry since production began at its plant in 1999. The company is a wholly-owned subsidiary of Calumite Ltd (Scunthorpe) which has been producing Calumite since 1969. Calumite Sro has helped the growth in glassmakers' use of Calumite as part of their melting batch. In this article the authors outline progress to date.

Author
Un-named
Origin
Unknown
Journal Title
Glass Int November 2007 47-48
Sector
General
Class
G 3429