Cascada: Surface Modification Developed For Glass Showers

Cascada, is a newly developed hydrophobic coating for use on glass showers. Test methods had to be developed and existing "standard test methods" had to be adapted by the manufacturer in order to measure Cascada's high wear resistance using a reasonable scale.