Canadian Recycling Update

A survey conducted in 1992 by Statistics Canada has found glass containers to have the best recovery rate for all types of packaging in Canada. More than 60% of container glass is being reused in Canada.

Author
Un-named
Origin
Unknown
Journal Title
American Glass Review 115 3 August 1994 8
Sector
Container glass
Class
C 716

Request article (free for British Glass members)

Canadian Recycling Update
American Glass Review 115 3 August 1994 8
C 716
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
17 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.