Camera-Based Weight Control Provides Precise Gob Management

Plunger cylinder sensor technology is a well-proven function of the Heye Process Control system, supervising and adjusting press-blow and NNPB production processes. Until how, these benefits have not been possible for glass container production via a blow-blow operation. According to Heye International, a Gob Master system closes this gap, ensuring that sophisticated process control integrates the benefits of visual gob measurement.

Author
Un-named
Origin
Unknown
Journal Title
Glass Worldwide Nov-Dec 2019 78
Sector
Container glass
Class
C 6214

Request article (free for British Glass members)

Camera-Based Weight Control Provides Precise Gob Management
Glass Worldwide Nov-Dec 2019 78
C 6214