Calp Back Into Profit In 2004

Italian crystal products manufacturer CALP posted a net profit of EUR 670,000 for 2004, it was reported on 2 May/05. The company closed 2003 with a net loss of EUR 6.54M. Net revenue in 2004 stood at EUR 79.9M up 21.08% year-on-year, the company said in a statement.