Bystronic Glass: Entry Model For Industrial Ig Production

Bystronic glass has recently launched the comfort line to the European Market designed for the production of insulating glass. Bernhard Schmitt, Managing Director of Bystronic glass in Neuhausen-Hamberg, Germany states that, "Working with the line is comfortable, quick and precise providing the ideal entry into solution for industrial insulating glass production." He explains: "At the same time, the comfort line allows us to reach out to customers who are searching for an inexpensive opportunity to expand their insulating glass production capacity." 800 gas-filled insulating glass units can be produced in rectangular or shaped formats on the quick line per shift.

Author
Un-named
Origin
Unknown
Journal Title
www.Glassonline.com March 2012
Sector
Flat glass
Class
F 3256

Request article (free for British Glass members)

Bystronic Glass: Entry Model For Industrial Ig Production
www.Glassonline.com March 2012
F 3256
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.