Breakthrough In Infra-Red Trend Analysis

In this article some preliminary results of a completely new system for infrared trend analysis, known as ITAS 2000 is described.

Author
Ing D Troost Et Al
Origin
Tce Consultancy & Engineering
Journal Title
International Glass Review Spring/Summer 1996 125-127
Sector
Container glass
Class
C 947

Request article (free for British Glass members)

Breakthrough In Infra-Red Trend Analysis
International Glass Review Spring/Summer 1996 125-127
C 947
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.