Boronizing As A New Method For Treatment Of Steel For One-Coat Enameling

An efficient method is developed for preparing steel surface before single-coat enameling which involves boronzing in solid solutions, making it possible to shorten the process of pretreatment of the metal and make it more efficient without using special equipment.