Boron Oxide And Lead Migration

This paper deals especially with the effect of boron oxide on lead leaching and other important parameters of lead crystal glasses containing 24% by weight of Pb0 or more.

Author
M Rada & M Petera
Origin
Inst Chem Techn, Prague
Journal Title
Int Cryst Fed 1998 70-85
Sector
Domestic glass
Class
D 405