The Benefits Of Combustion Air Staging

As a response to environmental concerns, the reduction of stack emissions is just one of the many advantages of oxy-fuel firing.

Author
J Latter
Origin
Combustion Tec, Usa
Journal Title
Gpti 1998 35-36, 38-39
Sector
General
Class
G 1833