Beneficiation Of Glass Sand - A Review

The massive expansion of the glass industry in India, especially sheet glass has led to a tremendous growth in the demand for silica sand. Reserves of superior quality sand are fast depleting. Thorough beneficiation of the available inferior quality sand is fast becoming a necessity. This article reviews beneficiation methods and looks at the technology available.