Bendable Silver-Based Low Emissivity Coating On Glass

A detailed study of a multilayer design for a temperature-resistant low emissivity and highly conductive coating is reported.

Author
J Sczcrbowski, A Dietrich, K Hartig
Origin
Unknown
Journal Title
Proc Spie Int Soc Opt Engrs 1987 823 21-27
Sector
Flat glass
Class
F 117