Bekaert: Increased Effciencies And Cost Savings For Display Manufacturers

In this article, Bekaert explains how the introduction of high performance rotatable ITO (indium-tin-oxide) targets and advances in sputter hardware, such as rotatable magnetrons, will shape the future of the display market. This is made possible, says the firm, by reducing the "Total Cost of Ownership".

Author
W De Bosscher Et Al
Origin
Bekaert Advanced Coatings
Journal Title
Glass Coatings 1/2006 20-23
Sector
Flat glass
Class
F 1999