Basic Glass Strength Factors

The basis for the factors used to adjust annealed glass strengths for use of heat-strengthened and fully toughened glass are discussed.

Author
J E Minor
Origin
University Of Missouri-Rolla
Journal Title
Glass Digest August 15 1990 52-56
Sector
Flat glass
Class
F 237