Basic Flow Pattern And Its Variation In Different Types Of Glass Tank Furnaces

The molten glass current in tank furnaces was studied by physical modelling. The basic flow pattern was divided into batch, melting, stagnant buffer, refining and conditioning regions. Every region and its special function are discussed in this paper.