Automatic Lines For Ampoules And Vials

Ariste started its activity in 1948 and is specialised in automatic lines for ampoules and vial processing. In this article, the author presents two new lines which adopt new technologies for dimensional controls, cutting of ampoules, vitrification ovens, packaging and, above all, transfer robots.

Author
M Buttinoni
Origin
Ariste
Journal Title
Glass Machinery Plants & Accessories No 3 1995 112-114