Automatic High Performance Glass Pressing Lines And Centrifuges/Spinning Machines For The Production Of Tableware

In this paper the author looks at some of the latest editions made by Walter Co., of Germany, a manufacturer of complete hollow ware production lines that has supplied industry for over 50 years. The company's technical expertise spans all areas of glassmaking and they are active in over 100 countries supplying forehearths, feeders, automatic glass pressing machines, fire polishing machines, transport and handling systems, cross conveyors, and push bar stackers.

Author
P Gottmann
Origin
J Walter Co, Germany
Journal Title
Kanch February 1999 33-47
Sector
Domestic glass
Class
D 380

Request article (free for British Glass members)

Automatic High Performance Glass Pressing Lines And Centrifuges/Spinning Machines For The Production Of Tableware
Kanch February 1999 33-47
D 380
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
14 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.