Automatic Glass Examination Using Retro-Reflective Laser Scanning

The advantages of retro-reflective laser systems over traditional technologies for inspection of flat glass are discussed.

Author
J F Claridge
Origin
Image Automation Limited
Journal Title
Glass Production Technology International 1991 229-234
Sector
Flat glass
Class
F 292