Automated Hot End Inspection And Monitoring

The I-Sight 20/20 hot end inspection system has been designed for inspecting glass containers at the hot end of glass factories to provide more immediate feedback on the production process. The development of the system was carried out with the collaboration of several glass manufacturers and has undergone successful beta-testing at hot end lines.