Atmospheres In Glass Melts: Challenges And Benefits

When glass is in the molten state, gases and water in the melt atmosphere can plague unaware glassmakers with problems, or, when understood, can enhance glass products. Industry scientists examine the effect of atmospheress on commercial glass melts and define the challenges to theoretical researchers.

Author
F Woolley
Origin
Corning Inc, Usa
Journal Title
The Glass Researcher 10Th Anniversary Collection 1986/96 16-17
Sector
General
Class
G 2687