Assessing The Thermal Safety Of Flat Glass Subjected To Solar Radiation: Part 1: Edge Strength

It has been shown that measurements of edge strength under 4-point loading enables assessments of thermal safety, based on experience with clean-cut edges, to be extended to include arrissed edges. Some of the results reported are from work carried out by BGIRA.