The Applications Of Mossbauer Spectroscopy To The Study Of Inorganic Oxide Glasses

The data obtained during the last decade on borate, silicate and phosphate glasses by the Mossbauer technique are reviewed with reference to the literature.

Author
S S Sekhon, R Kamal
Origin
Guru Nanek Dev University, Punjabi University
Journal Title
Phsyics And Chemistry Of Glasses 1988 29 4 157-167
Sector
General
Class
G 139

Request article (free for British Glass members)

The Applications Of Mossbauer Spectroscopy To The Study Of Inorganic Oxide Glasses
Phsyics And Chemistry Of Glasses 1988 29 4 157-167
G 139