Application Of Optical Testing Procedures To Quality Control Of Flat Glass

Optical testing procedures applied to the quality assurance of float glass production are described. The identification of point defects, testing for optical quality, surface flatness and residual stress are discussed briefly.

Author
J Bretschneider
Origin
Flachglas Ag
Journal Title
Glastech Ber 1988 61 6 172-175