Application Of Microwaves In Glass Conditioning

Results from tests on several forehearths are presented. The effects of microwaves on chemical and thermal homogeneity can be observed. Glasses exposed to microwave energy include borosilicate, soda-lime, barium and lead crystal.

Author
P Vilk
Origin
Bh-F Engineering, Uk
Journal Title
65Th Conference On Glass Problems 2004 63-70
Sector
General
Class
G 2992