Apple Computer Inc Retail Store - All Glass Staircase And Bridge: A Technical Review Of Innovative Design And Fabrication Techniques Utilised

In this paper the author describes the techniques developed and adopted for the connection of laminated glass treads to supporting glass structure for a stair and bridge in a retail environment.