Ansi Z97.1 - Safety Glazing Materials Used In Buildings

A new version of ANSI (American National Standards Institute) Z97.1 "Safety Glazing Materials Used in Buildings" was released in 2004. The standard establishes the specifications for glazing materials used for all building and architectural purposes. You can order a copy from the ANSI website, www.ansi.org - priced at US$60.