Analytical Development Of Cast Iron Enamelling

This paper describes selected work on an EC CRAFT project (ADCIE) on enamelling of cast iron. An expert system has been developed for use as a diagnostic tool in identifying enamelling defects and providing remedial solutions. The routine for boil defects is described and the results of investigative work on the causes of boil defects given.