Analysis And Modelling Of Glass Melting

In overlooking the glass melting process, three research activities in the field may be noticed: Improvement and new ways of glass melting; automatic process control by models, and identification and elimination of glass melting defects. This paper presents and evaluates some intersting trends in the above-mentioned areas.