All-Electric Furnace Melting Fluor-Opal Glass

Refractory wear and corrosion in an electric furnace melting fluor-opal glass were investigated. The influences on the campaign of the furnace are also discussed. This paper looks at ways of prolonging the campaign and saving energy.