Air Convection Tempering Furnaces

The production of tempering and bending furnaces has established the Swiss company Cattin Machines as a well-known supplier to the automotive glass industry. This paper reviews a new type of horizontal convection furnace for tempering flat or bent architectural glass as well as for inclsuion in the production line of bent tempered automotive glass.