Ag/M-Seed/Azo/Glass Structures For Low-E Glass: Effects Of Metal Seeds

In this work, continuous and conductive ultrathin Ag films with highly infrared reflective and highly visible transmittance were achieved using several metal seeds (Ti, Nb, Cr, Ni, Mo, Pt, Cu and Ru), having ~1-2nm in thickness, deposited between Ag and dielectric AZO layers on glass substrate by magnetron sputtering with confocal target geometry. The optical properties in the visible and infrared ranges and conductivity of Ag/M-seed/AZO/glass structures were compared in order to determine the influence of the seeds. It was observed that all M-Seeds increased both visible transmittance and infrared reflectance. But also, it was shown that Nb and Ti seed layers which help on coalesced of Ag and AZO layers are more effective on the electro-optical characteristics of the Ag thin films than the other seeds.

Author
N A Sonmez Et Al
Origin
Gazi University, Turkey
Journal Title
Int J Appl Glass Sci 9 2018 383-391
Sector
Flat glass
Class
F 4086

Request article (free for British Glass members)

Ag/M-Seed/Azo/Glass Structures For Low-E Glass: Effects Of Metal Seeds
Int J Appl Glass Sci 9 2018 383-391
F 4086
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.