Advantages Of Modular Electronics For Large Area Sputter Coatings

Magnetron sputtering is the most used method for thin film deposition, supported by ease in scaling up to large dimensions, high deposition rate, good thickness control, layer quality, uniformity and the wide variety of materials to be deposited. Modular electronics, presented in this paper by Bekaert, can provide optimal flexibility, thus maximising process stability and sputter rate. Further integration with the magnetron, magnetic system, target and gas distribution can improve overall control and flexibility.

Author
Un-named
Origin
Unknown
Journal Title
Glass Coatings 3/06 17-21
Sector
Flat glass
Class
F 2154

Request article (free for British Glass members)

Advantages Of Modular Electronics For Large Area Sputter Coatings
Glass Coatings 3/06 17-21
F 2154
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.