Advantages Of Boron In Glass Mineral Wool Insualtion

Glass Technology Services, the independent technical subsidiary of British Glass (UK Trade Federation), recently undertook a review on the role of boron in glass mineral wool insulation. The report explored the important benefits boron brings to glass mineral wool insulation, a borosilicate glass, of which it is a major structural component.