Adding Value To Glass

Johnson Matthey Colour Technologies supplies colour & precious metal inks for decorative & technical applications to glass & ceramics. The company's market position is built on over 200y experience. Many of the challenges affecting glass decoration are not unique to this industry: market conditions are increasingly competitive, legislative & environmental pressures drive technological innovation & the globalisation of markets offers both opportunities & threats. The decoration of glass allows customers to differentiate & add value to their product, whether for functional or aesthetic reasons. Glass enamels & precious metal inks still offer the best technical performance for many applications. In this article the author outlines the range of colours & precious metal inks that are available for the decoration of different types of glass.

Author
P Cartlidge
Origin
Johnson Matthey, Uk
Journal Title
Glass Worldwide Sept-Oct 2007 78-79
Sector
Domestic glass
Class
D 1055

Request article (free for British Glass members)

Adding Value To Glass
Glass Worldwide Sept-Oct 2007 78-79
D 1055
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.