Adding Lithium Minerals Can Reduce Melting Costs

The use of glass grade spodumene has been shown to provide economic benefits in the melting of various types of glass.

Author
D J Kingsworth
Origin
Lithium Australia Ltd
Journal Title
Glass Industry March 1988 18-25
Sector
General
Class
G 162

Request article (free for British Glass members)

Adding Lithium Minerals Can Reduce Melting Costs
Glass Industry March 1988 18-25
G 162
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.