Absorption And Fluorescence Of Trivalent Europium In Borate Glasses

The absorption and fluorescence spectra and fluorescence lifetimes of trivalent europium ions were investigated in a variet of borate glasses at room temperature. The spectral characteristics were related to various europium-glass interactions and discusses with reference to changes in strucutre occuring in the host glass.

Author
P.K. Gallagher Et Al.
Origin
Unknown
Journal Title
Physics And Chemistry Of Glasses 1965 6 (3) June 95-103